SAE 4617/4615 EN34 Hot Forged Steel Round Bar
1: BS EN34 Steel Introduction
EN34 is a 2% nickel, molybdenum case hardening steel grade. Combining good core strength, toughness and fatigue resistance this grade can be case hardened up to 60HRc. EN34 is suitable for applications requiring wear resistance and shock resistance. It offers good core strength and impact properties with little temper brittleness.
EN34 steel Stock in warehouse
2: 4615 Quality Standard
3: BS EN34 Steel Equivalent
Country | China | Japan | Germany | USA | British |
Standard | GB GB/T 3077 | JIS JIS G4105/JIS | DIN (W-Nr.) EN 10250 | AISI/ASTM ASTM A29 | BS BS 970 |
Grade | / | / | / | 4615 / 4617 | EN34 / 665M17 |
4: BS EN34 Steel Chemical Composition
Grade | C | Si | Mn | P | S | Mo | Ni |
EN34 / 665M17 | 0.14-0.20 | 0.10-0.35 | 0.35-0.75 | ≤ 0.035 | ≤ 0.040 | 0.20-0.30 | 1.50-2.00 |
4615 / 4617 | 0.13-0.18 | 0.15-0.30 | 0.45-0.65 | ≤ 0.035 | ≤ 0.040 | 0.20-0.30 | 1.65-2.00 |
5: BS EN34 Steel Mechanical Properties
The mechanical properties mainly include tensile strength, yield strength, elongation, area or reduction, hardness, impact value, non-metalic inclusion etc. Different heat treatment, the mechanical properties will be different, such as normalized, tempered, QT. If you want to know the properties, please kindly contact the salesman.
6: BS EN34 Steel Overviews
Size | Round | Dia 6-1200mm |
Plate/Flat/Block | Thickness 6mm-500mm | |
Width 20mm-1000mm | ||
Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
Delivery condition | Forged; Hot rolled; Cold drawn | |
Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
Payment terms | T/T;L/C;/Money gram/ Paypal | |
Trade terms | FOB; CIF; C&F; etc.. | |
Delivery time | 30-45 days |
7: BS EN34 Steel Application
BS EN34 is suitable for shafts, gears, transmission parts, camshafts and cams, cam shafts connecting rods crankshafts gears.
8: BS EN34 Carburising / Case Hardening
Carburising and case hardening will give a hard wear resisting surface and a tough core strength to the steel. EN34 is suited for carburising and case hardening. Surfaces must be free from dirt and grease, and of low sulphur content. Case hardening can be carried out in salt baths with selected content depending on the type of salt and the depth of penetration required. Other considerations during the heat treatment process include the type of furnace, quenching medium and work piece transfer facilities. Time, temperatures and salt selection will be advised by your heat treatment provider.
9: BS EN34 Steel Heat Treatment
Heat treatment temperatures, including rate of heating, cooling and soaking times will vary due to factors such as the shape and size of each EN34 steel component. Other considerations during the heat treatment process include the type of furnace, quenching medium and the work piece transfer facilities. Please consult your heat treatment provider for full guidance on heat treatment of EN34 case hardening steel.
10: BS EN34 Steel Tolerance
Diameter(mm) | Tolerance | |||||
Forged Steel Round Bar | 80-600 | Black Surface:0~+5 | Rough Machined or Turned:0~+3 | |||
650-1200 | Black Surface:0~+15 | Rough Machined or Turned:0~+3 | ||||
Hot Rolled Steel Round Bar | 16-310 | Black Surface:0~+1 | Peeled:H11 | |||
Cold Drawn Steel Round Bar | 6-100 | Black Surface:H11 | Peeled:H11 |
10: BS EN34 Delivery condition
Usually the delivery condition is hot forged or rolled, annealed, rough turned for hot forged or hot rolled bar.
For hot forged or hot rolled plate, usually the delivery condition is hot forged, annealed, milled surface or hot rolled, annealed, black surface.